Wood seasoning is the controlled drying of freshly sawn wood to a moisture content suitable for its intended service. It reduces the movement and distortion that would otherwise occur after boards are cut to size, joined, or installed. Air seasoning uses the surrounding air to carry away moisture. A kiln controls temperature, humidity, and air movement and can bring wood to a lower, more consistent moisture content. This article follows the U.S. Forest Products Laboratory's Wood Handbook for drying and measurement.[1]

Stacks of sawn boards beside lumber-mill buildings
Lumber stacked at the Bloedel-Donovan mill in Washington state, circa 1922-1923. The archive identifies the load as cargo for a dry kiln. Photograph from University of Washington Libraries, Special Collections (U.S. public domain).

Moisture and movement

Moisture content for lumber is the mass of water in the wood divided by the mass of the wood after oven drying, expressed as a percentage. Wood contains both free water in its cavities and water bound in its cell walls. Shrinkage takes place chiefly as the cell walls lose water below the fiber saturation point. Wood normally shrinks more across the grain than along it, and more tangentially to the growth rings than radially across them. These differences can cause a board to cup or change shape as it dries.[2][1]

Wood exchanges moisture with the surrounding air even after seasoning. At a steady temperature and relative humidity it tends toward an equilibrium moisture content. Outdoor air may leave lumber suitable for one use while still too moist for a heated interior. Set the target for the service conditions and product requirements before choosing a drying method. For comparison, the Forest Products Laboratory reports that hardwood for furniture, flooring, cabinets, and millwork is usually dried to 6% to 8%. This is a typical production range for those products.[2][1]

Air-drying a stack

Choose a firm, well-drained site with space for air to move around the pile. Raise the stack off the ground on level supports. Sort the boards by thickness and, where practical, by species and drying behavior. Different thicknesses in one layer create uneven bearing on the boards and spacers above. Leave openings for air to enter the stack and protect it from rain with a roof or supported cover that leaves the sides open.[3]

Lay straight, dry wooden spacers, called stickers, across the width of the pile between each layer. Use uniform thickness so the boards have even support. Place stickers near board ends and at intervals appropriate to board thickness and stiffness. Align rows of stickers vertically over the base supports to transmit weight through the stack without bending unsupported board spans. If boards have mixed lengths, arrange them so shorter boards also have support close to their ends. Keep the stack stable and check that it remains level as the ground and stock change.[3]

Wood loses moisture quickly through exposed end grain. A moisture-resistant end coating can help reduce end checks and splitting, but it must be applied to freshly trimmed green ends before any checking has started. Intense drying can also produce surface checks, while warm, humid and still conditions favor fungal stain. Inspect periodically for rain exposure, bent supports, blocked air passages, stain and checks. Improve circulation or shelter as the signs warrant. Drying rate varies greatly with species, thickness, season, and climate, so use measurements to decide when the stack can be moved or used.[3][1]

Measuring moisture content

Method Use and limitations
Oven-dry test Weigh a representative cut sample promptly, dry it to constant mass, then subtract its dry mass from the initial mass, divide by the dry mass, and multiply by 100 for a percentage. This provides a direct estimate but requires cutting a specimen and takes longer than an electrical reading. Take specimens free of knots and other irregularities at least 500 mm (20 in.) from board ends, which gain and lose moisture faster than the rest of the board.[1]
Resistance meter with pins Measures electrical resistance between inserted electrodes. Insulated pins sense at their exposed tips, so measuring at different depths can reveal a wetter core. Bare pins can be dominated by the wettest material along the insertion path.[1]
Dielectric or pinless meter A surface-contact sensor estimates moisture without making pinholes. The surface layers influence the result strongly, so the reading can miss a wetter interior. Select the instrument's species or density setting as directed.[1]

Measure several boards from different parts of the pile, including stock sheltered in the interior, before accepting the lot. Record board thickness, the meter settings, and the locations and depths of readings. Follow the manufacturer for pin orientation and applicable species and temperature corrections. The Forest Products Laboratory describes about 30% as the upper end of the reliable range for ordinary resistance and dielectric meters. Readings above that point are qualitative. If readings differ greatly between the faces and the core or between boards, investigate the variation before declaring the stack ready.[1]

Readiness and storage

A covered outdoor stack can stop losing moisture while still too damp for a particular job. The Forest Products Laboratory gives 12% to 15% as the minimum moisture content of thoroughly air-dried lumber for much of the United States. For example, air-seasoned boards intended for furniture in a heated room may need further controlled drying and time to acclimate before final machining. Protect dried lumber from rain and humid storage and check moisture again before use. A dry reading does not show that boards have no internal checks or residual drying stresses, or that they meet a structural grading or product requirement.[1][3]

See also

References

  1. ↑ 1.0 1.1 1.2 1.3 1.4 1.5 1.6 1.7 1.8 Bergman, Richard (2021). Drying and control of moisture content and dimensional changes. Wood Handbook: Wood as an Engineering Material, Ch. 13. USDA Forest Service, Forest Products Laboratory, FPL-GTR-282. Retrieved 21 November 2026.
  2. ↑ 2.0 2.1 Glass, Samuel V. and Zelinka, Samuel L. (2021). Moisture relations and physical properties of wood. Wood Handbook: Wood as an Engineering Material, Ch. 4. USDA Forest Service, Forest Products Laboratory, FPL-GTR-282. Retrieved 21 November 2026.
  3. ↑ 3.0 3.1 3.2 3.3 Forest Products Laboratory (1999). Air Drying of Lumber. USDA Forest Service, FPL-GTR-117, especially the sections on pile protection, end coatings and stickering. Retrieved 21 November 2026.