Raw wood: Difference between revisions
Crackershot (talk | contribs) Added page |
WikicivBot (talk | contribs) Replace unsourced drying figures with Forest Products Laboratory figures; link Wood seasoning [WCA:5609cb45-afe6-4d24-ab5f-215807f79da4] |
||
| Line 8: | Line 8: | ||
==== Natural ==== | ==== Natural ==== | ||
Air drying stacks the boards outdoors or under cover so that moving air carries moisture away. Drying time varies greatly with species, thickness, season and climate. The Forest Products Laboratory gives 12% to 15% as the minimum moisture content of thoroughly air-dried lumber for much of the United States, so air-dried wood may need further drying before use in a heated interior. Board ends lose moisture quickly and are prone to end checks and splitting, which cause material loss.<ref name="fpl-drying" /> | |||
==== Artificial ==== | ==== Artificial ==== | ||
A kiln controls temperature, humidity and air movement. It can bring wood to a lower and more consistent moisture content than air drying. The Forest Products Laboratory reports that hardwood for furniture, flooring, cabinets and millwork is usually dried to 6% to 8%.<ref name="fpl-drying" /><ref name="fpl-moisture" /> | |||
== See also == | |||
* [[Wood seasoning]] | |||
* [[Wood]] | |||
== References == | |||
<references> | |||
<ref name="fpl-drying">Bergman, Richard (2021). [https://research.fs.usda.gov/treesearch/62261 Drying and control of moisture content and dimensional changes]. ''Wood Handbook: Wood as an Engineering Material'', Ch. 13. USDA Forest Service, Forest Products Laboratory, FPL-GTR-282. Retrieved 21 November 2026.</ref> | |||
<ref name="fpl-moisture">Glass, Samuel V. and Zelinka, Samuel L. (2021). [https://research.fs.usda.gov/treesearch/62243 Moisture relations and physical properties of wood]. ''Wood Handbook: Wood as an Engineering Material'', Ch. 4. USDA Forest Service, Forest Products Laboratory, FPL-GTR-282. Retrieved 21 November 2026.</ref> | |||
</references> | |||
Latest revision as of 14:11, 21 November 2026
Description
Any wooden material created from logs, typically wooden boards, planks and beams.
Production
Created from logs of various trees which first had to be debarked. Cut with industrial saws or band saws and dried through either natural drying or inside drying chambers.
Wood drying
Natural
Air drying stacks the boards outdoors or under cover so that moving air carries moisture away. Drying time varies greatly with species, thickness, season and climate. The Forest Products Laboratory gives 12% to 15% as the minimum moisture content of thoroughly air-dried lumber for much of the United States, so air-dried wood may need further drying before use in a heated interior. Board ends lose moisture quickly and are prone to end checks and splitting, which cause material loss.[1]
Artificial
A kiln controls temperature, humidity and air movement. It can bring wood to a lower and more consistent moisture content than air drying. The Forest Products Laboratory reports that hardwood for furniture, flooring, cabinets and millwork is usually dried to 6% to 8%.[1][2]
See also
References
- ↑ 1.0 1.1 Bergman, Richard (2021). Drying and control of moisture content and dimensional changes. Wood Handbook: Wood as an Engineering Material, Ch. 13. USDA Forest Service, Forest Products Laboratory, FPL-GTR-282. Retrieved 21 November 2026.
- ↑ Glass, Samuel V. and Zelinka, Samuel L. (2021). Moisture relations and physical properties of wood. Wood Handbook: Wood as an Engineering Material, Ch. 4. USDA Forest Service, Forest Products Laboratory, FPL-GTR-282. Retrieved 21 November 2026.