Pottery: Difference between revisions
minor, added beeswax as a sealant. need to add how to find suitable material. |
No edit summary |
||
| Line 1: | Line 1: | ||
[[File:Mycenaean pottery, Kanellopoulos Museum, 225118.jpg|thumb|Mycenaean vases. Kanellopoulos Museum at Athens.]]'''Pottery''' is the process and the products of forming vessels and other objects with [[clay]] and other [[ceramic]] materials, which are fired at high temperatures (600–1600 °C) to give them a hard and durable form. | [[File:Mycenaean pottery, Kanellopoulos Museum, 225118.jpg|thumb|Mycenaean vases. Kanellopoulos Museum at Athens.]]'''Pottery''' is the process and the products of forming vessels and other objects with [[clay]] and other [[ceramic]] materials, which are fired at high temperatures (600–1600 °C) to give them a hard and durable form. | ||
== Uses == | |||
Pottery is widely used for cookware, storage, and tooling. Art pieces may also be formed with clay. | |||
== Materials needed == | == Materials needed == | ||
| Line 8: | Line 11: | ||
* Optionally: a pottery wheel and [[ceramic glaze]] | * Optionally: a pottery wheel and [[ceramic glaze]] | ||
== Crafting | == Identify and extract clay == | ||
Where to find clay? | |||
Wetlands: '''riverbanks''', lakeshores, or clayey areas ('''sticky soil''' when it rains, cracks when dry). | |||
Geological layers: Cliffs, quarries, or grey/yellow soils ('''avoid sandy soils'''). | |||
Simple test: Take a sample, wet it and mix. Make into a '''coil and twist it''' around your finger. If it does not crack, it is clay. | |||
Extraction: | |||
Dig to a depth of 30-50 cm (1-2 elbow to fist length) to avoid impurities. | |||
Recover 5-10 kg for a first test. | |||
== Clean and prepare clay == | |||
=== Remove impurities : === | |||
# Work the clay with water and remove stones and roots. | |||
=== Decanting: === | |||
# Mix the clay with a lot of water in a bucket or basin. | |||
# Leave for 24 hours: heavy particles (sand) sink to the bottom, while the clay remains in suspension. | |||
# Collect the cloudy water (clay) and discard the sandy deposit. | |||
# Spread the mud on a cloth or plate to evaporate excess water. | |||
# When the clay is malleable (modeling clay consistency), it's ready. | |||
== Crafting instructions == | |||
Pottery can be created using many different methods. Here will be covered: Pinch, coil, and turned pottery. After the pottery is formed, the process is the same. | Pottery can be created using many different methods. Here will be covered: Pinch, coil, and turned pottery. After the pottery is formed, the process is the same. | ||
=== Pinch Pottery === | |||
# With a ball of clay or other pottery medium, gradually pinch and shape into desired form. | # With a ball of clay or other pottery medium, gradually pinch and shape into desired form. | ||
=== Coil Pottery === | |||
# Begin with a flat base of clay, serving as the bottom of the pottery. | # Begin with a flat base of clay, serving as the bottom of the pottery. | ||
# Roll a coil of clay and fuse it on top of the base, tracing the perimeter. Watered down clay, called slip, is used. | # Roll a coil of clay and fuse it on top of the base, tracing the perimeter. Watered down clay, called slip, is used. | ||
| Line 22: | Line 52: | ||
# Coils may be smoothed over to finalized its form. | # Coils may be smoothed over to finalized its form. | ||
=== Turned pottery === | |||
While turning pottery, it is important that hands are always kept wet to lubricate the clay. | While turning pottery, it is important that hands are always kept wet to lubricate the clay. | ||
| Line 34: | Line 64: | ||
# Once the clay has dried to the point to leather-hardness (firm, and not sticky) it may be trimmed. | # Once the clay has dried to the point to leather-hardness (firm, and not sticky) it may be trimmed. | ||
== Firing to ceramic == | |||
When clay is worked into pottery, it is still wet and will dissolve in water. To make it more durable, it must be fired into ceramic. | |||
# Allow the pottery to slowly dry out completely, covered with a damp cloth. Too rapid of drying may cause warping or cracking. | |||
# The bone-dry pottery can now be bisque-fired at 850–1000°C (1560–1830°F) for about 8 to 14 hours depending on size and shape. This can be done in a hole in the ground or in a kiln. | |||
# The pottery will now be ceramic, but will be porous and may not hold water. The pottery can now be glazed and fired again at 1040–1100°C (1900–2010°F) for earthenware glaze or 1200–1300°C (2190–2370°F) for stoneware glaze for about 6 to 10 hours depending on size and shape. | |||
Ceramic pottery can also be made non porous by using wax, such as beeswax. Apply when the pottery is still warm from the firing (not too hot or it may catch fire) and as the wax melts it will be absorbed by the ceramic, making it watertight. | Ceramic pottery can also be made non porous by using wax, such as beeswax. Apply when the pottery is still warm from the firing (not too hot or it may catch fire) and as the wax melts it will be absorbed by the ceramic, making it watertight. | ||
==Dependencies== | ==Dependencies== | ||
Revision as of 09:45, 10 May 2025

Pottery is the process and the products of forming vessels and other objects with clay and other ceramic materials, which are fired at high temperatures (600–1600 °C) to give them a hard and durable form.
Uses
Pottery is widely used for cookware, storage, and tooling. Art pieces may also be formed with clay.
Materials needed
- Clay, or other pottery medium
- A source of heat, in the form of fuel (wood, coal or gas) or electricity through a resistance
- Optionally: a kiln for containing the heat and achieving higher temperatures
- Optionally: a pottery wheel and ceramic glaze
Identify and extract clay
Where to find clay?
Wetlands: riverbanks, lakeshores, or clayey areas (sticky soil when it rains, cracks when dry).
Geological layers: Cliffs, quarries, or grey/yellow soils (avoid sandy soils).
Simple test: Take a sample, wet it and mix. Make into a coil and twist it around your finger. If it does not crack, it is clay.
Extraction:
Dig to a depth of 30-50 cm (1-2 elbow to fist length) to avoid impurities.
Recover 5-10 kg for a first test.
Clean and prepare clay
Remove impurities :
- Work the clay with water and remove stones and roots.
Decanting:
- Mix the clay with a lot of water in a bucket or basin.
- Leave for 24 hours: heavy particles (sand) sink to the bottom, while the clay remains in suspension.
- Collect the cloudy water (clay) and discard the sandy deposit.
- Spread the mud on a cloth or plate to evaporate excess water.
- When the clay is malleable (modeling clay consistency), it's ready.
Crafting instructions
Pottery can be created using many different methods. Here will be covered: Pinch, coil, and turned pottery. After the pottery is formed, the process is the same.
Pinch Pottery
- With a ball of clay or other pottery medium, gradually pinch and shape into desired form.
Coil Pottery
- Begin with a flat base of clay, serving as the bottom of the pottery.
- Roll a coil of clay and fuse it on top of the base, tracing the perimeter. Watered down clay, called slip, is used.
- subsequent coils are fused to the layer below, building a vessel to desired shape.
- Coils may be smoothed over to finalized its form.
Turned pottery
While turning pottery, it is important that hands are always kept wet to lubricate the clay.
- On a pottery wheel, secure a lump of clay.
- While the wheel turns and with wet hands, cone the clay up and down to eliminate air bubbles and align the molecules of clay.
- Form a well in the clay until the desired thickness of the base is achieved.
- Pull the clay outwards to turn the well into the flat base.
- The walls can gradually be pulled up, having care to ensure the clay runs concentric to the wheel.
- After the shape is achieved, excess water is removed from inside and out to prevent disintegration.
- Removed from the wheel to dry.
- Once the clay has dried to the point to leather-hardness (firm, and not sticky) it may be trimmed.
Firing to ceramic
When clay is worked into pottery, it is still wet and will dissolve in water. To make it more durable, it must be fired into ceramic.
- Allow the pottery to slowly dry out completely, covered with a damp cloth. Too rapid of drying may cause warping or cracking.
- The bone-dry pottery can now be bisque-fired at 850–1000°C (1560–1830°F) for about 8 to 14 hours depending on size and shape. This can be done in a hole in the ground or in a kiln.
- The pottery will now be ceramic, but will be porous and may not hold water. The pottery can now be glazed and fired again at 1040–1100°C (1900–2010°F) for earthenware glaze or 1200–1300°C (2190–2370°F) for stoneware glaze for about 6 to 10 hours depending on size and shape.
Ceramic pottery can also be made non porous by using wax, such as beeswax. Apply when the pottery is still warm from the firing (not too hot or it may catch fire) and as the wax melts it will be absorbed by the ceramic, making it watertight.
Dependencies
See also
External links
- Clay pots suitable for preparing any food in the forest. - Pre Technology, 26 February 2021, YouTube